Items | Specifications | ||
Lithium-ion/Lithium Polymer | LiFePO4 | ||
Charge | Charging voltage(CC/CV)-1S | CC/CV:4.2V | CC/CV:3.6V |
Maximal continuous charging current | 2a(Max) | ||
Discharge | Maximal continuous discharging current | 2a(Max) | |
Low current consumption | Current consumption on operation | <20μA | |
Current consumption at power down | <0.1μA | ||
Cell-balance | Cell-balance detection voltage | / | / |
Cell-balance release voltage | / | / | |
Cell-balance current | / | / | |
Over-charge | Overcharge detection voltage | 4.25±0.025V | 3.900 ± 0.025V |
Overcharge release voltage | 4.15±0.05V | 3.800 ± 0.050V | |
Overcharge delay time | 0.5~2S | ||
Over-discharge | Overdischarge detection voltage | 2.50±0.062V | 2.00±0.080V |
Overdischarge release voltage | 3.0±0.075V | 2.30±0.100V | |
Overdischarge delay time | 100~300mS | ||
Discharge overcurrent | Discharge overcurrent detection voltage | 0.2±0.015V | 0.10±0.015V |
Discharge overcurrent delay time | 15~35ms | ||
Discharge overcurrent protection | 5±1a(adjustable) | ||
Release condition | Cut-off-load | ||
Short-circuiting protection | Load short-circuiting detection voltage | / | / |
Detection condition | Exterior short circuit | ||
Load short-circuiting detection delay time | 200~800μs | ||
Release condition | Cut-off-load | ||
Internal resistance | Static Drain-Source On-Resistance | <20mΩ(B- to P-) | |
Temperature | Wide range of operation temperature | 40 ~ + 85ºC | |
Storage Temperature Range | -40 ~ +125ºC | ||
Dimension | Φ9.8mm |